Close
 Indian J Med Microbiol  
 

Figure 4: Potentiodynamic polarization of titanium-based alloy exposed to the test solution containing various concentrations of Colgate™ gel [12 mg (1), 10 mg (2), 8 mg (3), 6 mg (4), 4 mg (5), 2 mg (6)] and control (7)

Figure 4: Potentiodynamic polarization of titanium-based alloy exposed to the test solution containing various concentrations of Colgate™ gel [12 mg (1), 10 mg (2), 8 mg (3), 6 mg (4), 4 mg (5), 2 mg (6)] and control (7)