 Indian J Med Microbiol  
 

Figure 2 :Representative SEM micrographs from the fractured surface of RfX post: (a) showing the metal reinforcement (M) surrounded by the glass fibers (F) (magnification, 131). (b) The magnified image shows the interaction between the glass fibers (F), the resin matrix (R), and the metal reinforcement (M) (magnification 1000)

Figure 2 :Representative SEM micrographs from the fractured surface of RfX post: (a) showing the metal reinforcement (M) surrounded by the glass fibers (F) (magnification, 131). (b) The magnified image shows the interaction between the glass fibers (F), the resin matrix (R), and the metal reinforcement (M) (magnification 1000)