In in-vitro evaluation of effect of different finish lines on marginal adaptation in metal-ceramic restorations under thermo-mechanical loading


Ridhima Gupta 
 Department of Prosthodontics, Institute of Dental Sciences and Technology, Modinagar, India

Correspondence Address:
Ridhima Gupta
Department of Prosthodontics, Institute of Dental Sciences and Technology, Modinagar
India

The aim of this study was to evaluate the marginal gap in terms of cement film thickness associated with shoulder, shoulder with 45° bevel, shoulder with 30° bevel and chamfer, under thermo-mechanical loading. Forty human mandibular molars were prepared and restored with ceramo-metal crowns. Teeth were thermo-mechanically loaded and vertically sectioned to evaluate the cement film thickness. Shoulder with 45° bevel provided the least marginal gap as compared with all the tested finish lines.


How to cite this article:
Gupta R. In in-vitro evaluation of effect of different finish lines on marginal adaptation in metal-ceramic restorations under thermo-mechanical loading.Indian J Dent Res 2011;22:608-610


How to cite this URL:
Gupta R. In in-vitro evaluation of effect of different finish lines on marginal adaptation in metal-ceramic restorations under thermo-mechanical loading. Indian J Dent Res [serial online] 2011 [cited 2021 Dec 3 ];22:608-610
Available from: https://www.ijdr.in/article.asp?issn=0970-9290;year=2011;volume=22;issue=4;spage=608;epage=610;aulast=Gupta;type=0