Close
 Indian J Med Microbiol  
 

Figure 1: Mean values and standard deviation of microhardness for VC and VW resins for the different polymerization cycles in water-bath and in microwave, before and after thermocycling. For each material, different upper case letters indicate statistically different values in the comparison among polymerization cycles (P < 0.05). For each material, different lower case letters indicate statistically different values before and after thermocycling (P < 0.05)

Figure 1:  Mean values and standard deviation of microhardness for VC and VW resins for the different polymerization cycles in water-bath and in microwave, before and after thermocycling. For each material, different upper case letters indicate statistically different values in the comparison among polymerization cycles (<i>P</i> < 0.05). For each material, different lower case letters indicate statistically different values before and after thermocycling (<i>P</i> < 0.05)