Indian Journal of Dental ResearchIndian Journal of Dental ResearchIndian Journal of Dental Research
HOME | ABOUT US | EDITORIAL BOARD | AHEAD OF PRINT | CURRENT ISSUE | ARCHIVES | INSTRUCTIONS | SUBSCRIBE | ADVERTISE | CONTACT
Indian Journal of Dental Research   Login   |  Users online: 5043

Home Bookmark this page Print this page Email this page Small font sizeDefault font size Increase font size         

 


 
ORIGINAL RESEARCH Table of Contents   
Year : 2009  |  Volume : 20  |  Issue : 2  |  Page : 180-184
Effect of repeated use on dentin bond strength of two adhesive systems: All-in-one and one-bottle


1 Department of Operative Dentistry , Dental Faculty, Shiraz University of Medical Sciences, Shiraz, Iran
2 Department of Pediatric Dentistry, Dental Faculty, Shiraz University of Medical Sciences, Shiraz, Iran

Correspondence Address:
Mahtab Memarpour
Department of Pediatric Dentistry, Dental Faculty, Shiraz University of Medical Sciences, Shiraz
Iran
Login to access the Email id

Source of Support: None, Conflict of Interest: None


DOI: 10.4103/0970-9290.52897

Rights and Permissions

Aims: To compare the effects of repeated use of two one-bottle adhesives with that of two all- in- one adhesives (with acetone solvent) on bond strength to dentin. Materials and Methods: A flat dentin surface was prepared on 120 bovine incisors using 600- grit abrasive pape. The teeth were randomly assigned into 12 equal groups. The four adhesive systems [Prime and Bond NT (P&B NT), One-Step Plus (OS), iBond (iB), and G-Bond (GB)] were used at baseline, after the lid of the container had been opened 30 times, and after it had been opened 60 times. Before each use of the adhesives, the lids of the containers were left open for 1 min. The resin composites were applied on the dentin in a cylindrical split mold. After thermocycling, shear bond strength test was performed with a universal testing machine at 1 mm/min. We used Kruskal-Wallis and Dunn tests for statistical analysis. Results: There was no statistically significant difference among bond strength (MPa) of the groups of P&B NT (31.9 4.6, 31.8 6.5, 26.1 6.7) and OS (33.2 5.1, 30.9 7, 29.3 5.9), respectively (P > 0.05). The mean of the bond strength of iB and GB after 60 times (15.3 4.1 and 12.2 3.9, respectively) was significantly lower than that of iB and GB at baseline (23.5 4.8 and 22.2 4.5, respectively) (P < 0.05). Conclusions: Repeated use (60 times) of the all-in-one adhesive led to a decline in the dentin bond strength. To avoid this problem it would be advisable to have containers with smaller amounts of adhesive or perhaps those with only a singe dose.


[FULL TEXT] [PDF]*
Print this article     Email this article

 
 Similar in PUBMED
   Search Pubmed for
   Search in Google Scholar for
 Related articles
  Citation Manager
 Access Statistics
  Reader Comments
  Email Alert *
  Add to My List *
 
 

 Article Access Statistics
    Viewed3443    
    Printed89    
    Emailed0    
    PDF Downloaded394    
    Comments [Add]    
    Cited by others 11    

Recommend this journal